Speciality Fibers

Multimode Fibers Singlemode Fibers Microstructured Fibers
Graded Index Fibers AS GE HCS Fibers
PCS Fibers ToBIAs  

 

Microstructured Fibers

Features
  • High numerical aperture possible
  • Radiation resistant
  • High Temperature resistant
  • (Biocompatible Material)
  • (Sterilizable by ETO, e-beam, gamma radiation)
  • Excellent chemical and abrasion resistance

Properties

  • Step Index Profile
  • Wavelength dependent numerical aperture 0.5 … 0.9
  • Operation wavelength range IR: 400nm … 2400nm
  • core diameter 5µm ... 600µm
Fiber Design
  • Pure fused silica (low OH-)
  • microstructured fused silica cladding
  • Acrylate coating (-40°C to 85°C)
  • Silicone resin coating (-40°C to 180°C)
  • Polyimide coating (-190°C to 385°C)

Options

  • Numerical apertures 0.5 … 0.9
  • Metal coating
  • Connectors with sealed ends (SMA, FC/PC, ST, DIN)
  • AS-Fiber cables
  • high temperatur acrylate -40°C to 200°C
  • Buffer Options:
  • Nylon (-40°C to 100°C)
  • ETFE (-200°C to 150°C)

 